Liu, Y.; Cadavid, D.; Ibañez,, M.; De Roo, J.; Ortega, S.; Dobrozhan, O.; Kovalenko, M.; Cabot, A. "Colloidal AgSbSe2 nanocrystals: Surface analysis, electronic doping and processing into thermoelectric functional-nanomaterial" Journal of Materials Chemistry C 4, 21, pp. 4756 - 4762. 2016 DOI: 10.1039/c6tc00893c